28/Nov/2017 | 4703210009 | Grade pulp rauma biobright wood, sulfate (insoluble sort) bleached softwood used for manufacturing sanitary napkins, the dry matter content 92.05% in rolls 81.6 sm (separate perforatsieyna 2 hour | FINLAND | RAUMACELL | ****** | CG 90% G / B | 20,378 | 16961,91 | ***** | 84 More Columns Available along with Company Name and Other Details etc. |
27/Nov/2017 | 4703210009 | Cellulose bleached sulphate softwood, mark: botnia nordic pine, papermaking sanbytovogo and hygienic, the estimated weight net (state standard 16932-93) -133 768 kg (90% sv.) - 540 svyazok__1.0__ composition of raw materials : pine (pinus silv | FINLAND | ABSENT | ****** | CG 90% G / B | 132,975 | 84769,78 | ***** |
24/Nov/2017 | 4703210009 | Standard sulfate softwood bleached pulp. in sheet size: 80cm h40sm. it is designed to test a pfi mill, lab pulp and paper industry .__ 1.0__ raw material composition: 60% of the fir, 40% pine. white 87% .tehnologiya: oxygen-ni | FINLAND | KCL | ****** | CG 90% G / B | 2 | 2248,27 | ***** |