24/Nov/2017 | 7601208002 | From raw aluminum secondary alloys, into ingots, ak5m2. himich.sostav al 90.72-95.34%, cu 0.8-1.57%, zn 0.81-0.98%, mg 0.01-0.49%, si 2.06-5.70%. in accordance with gost 1583-93, tensile strength no more 415mpa at 25 degrees. from. | JAPAN | ABSENT | *** | *** | 54,223 | 97059,17 | ***** | 84 More Columns Available along with Company Name and Other Details etc. |