31/Oct/2017 | 2701111000 | Black coal - anthracite, mark "am", fraction 13-25mm with utmost yield of volatile matter on a dry ash-free basis not more than 10.0% by weight: "trade house" coal technology "no am gost 51591-2000.. 3350 | RUSSIA | *** | 3350000,00 | KG | 3,350,000 | 360467,28 | ***** | 84 More Columns Available along with Company Name and Other Details etc. |
31/Oct/2017 | 2701111000 | Coal, anthracite, make a grade am (for industrial purposes, concentrates) with ultimate yield of volatile matter on a dry ash-free osnovu- 2.9% by weight having dimensions of 13-25 mm 404000-kg, gost 32464-2013:. sa "cep" hooke "trade zna | RUSSIA | *** | 404000,00 | KG | 404,000 | 52827,04 | ***** |
31/Oct/2017 | 2701111000 | Anthracite milling: carbonaceous material 1-3mm (mli 1-3mm); limit devolatilization in dry ashless-base 2.2%, moisture, 1.7%, 6.5%, ash, calorific value - 7850 kcal; total net weight 208 621 kg. tu 2162-001-80361189: uhl | RUSSIA | *** | 208621,00 | KG | 208,621 | 27642,28 | ***** |
31/Oct/2017 | 2701111000 | Carbonaceous material, fraction 1.0-3.0 mm and the angle stone - anthracite, c limit volatile content (on a dry ash free basis) 2.72% used as studio network carbon steel carbonaceous material fraction | RUSSIA | *** | 69303,00 | KG | 69,303 | 9819,75 | ***** |
31/Oct/2017 | 2701111000 | Carbonaceous material from coal anthracite with utmost volatile content (on a dry ash-free basis) of 3.7%, 3.8 mac.%, non-agglomerated, used at metallurgical plants in steelmaking uglerodosoderzhasch | RUSSIA | *** | 163200,00 | KG | 163,200 | 22,032 | ***** |
31/Oct/2017 | 2701111000 | Filter material anthracite "akvalat" ( "aqualat") on the other 2164-001-12148148-2009. 1.4-2.5mm fraction size, total volume - 1000 m3, acid-soluble 0.76% is contained. ash 5.80% is contained. moisture 2.6%; maximum output letuch.veschestv- 2.30%. filtration | RUSSIA | *** | 901184,00 | KG | 901,184 | 308959,17 | ***** |
30/Oct/2017 | 2701111000 | Anthracene limit volatile content of 10% (on a dry ash free basis) zola to 5% moisture to 10% ao "siberian anthracite" am-uhg tu 0325-010-00160301-2015 fraction 13-25 mm 1500000 | RUSSIA | *** | 1500000,00 | KG | 1,500,000 | 212,400 | ***** |
30/Oct/2017 | 2701111000 | Anthracene limit devolatilization 3 to 3.3% (on a dry ash free basis) moisture from 8 to 8.7% ashes from 3.7 to 4.6% moisture content of from 8 to 8.9% ashes from 6.8 to 8.6% moisture content of from 8.1 to 9 % ash from 3.7 to 4.7% of jsc "siberian anthracite" ako-uhg tu | RUSSIA | *** | 19280600,00 | KG | 19,280,600 | 1851572,61 | ***** |
27/Oct/2017 | 2701111000 | Coal anthracite grade "a" limit calorific value (on a wet ash-free basis) qsaf 7493-7530kkal / kg limit volatile content (on dry ash-free basis) vdaf 1, 9-3, 0%: ooo "section of east" but guests are not 32464-2013 70-100 mm 255 | RUSSIA | *** | 2559300,00 | KG | 2,559,300 | 191947,5 | ***** |
26/Oct/2017 | 2701111000 | Coal, anthracite, mark a, grade aa (for industrial purposes, concentrates) with ultimate yield of volatile matter on a dry ash-free osnovu- 2.8% by weight having dimensions of 50-100 mw, 263, 000-kg, gost 32464-2013:. sa "cep" hooke "zn sales | RUSSIA | *** | 263000,00 | KG | 263,000 | 39649,88 | ***** |